Skip links

Deburring and Polishing of Sintered Parts

Unique solution for finishing of sintered parts with satellite steel ball media and alkaline compound

  • Components : Sintered parts
  • Input Contamination : Burr and rust
  • Present Method : Vibratory finishing with ceramic media and diesel
  • Present cycle time : 60 minutes
  • Problems Faced : Inconsistency in finishing due to intricate shape. Frequent change of media due to different shapes
    • Labour work
    • Environmental concern due to use of diesel solvent

Solution provided by GALA:

  • Media used : Mix media of satellite and steel ball with alkaline compound
  • Compound : Corrosion free Alkaline compound specially developed for sintered parts
  • Output : Completely deburred and polished components
  • Cycle time : 30 Minutes
  • Advantages :
    1. Consistent Finishing
    2. No manual intervention. No change of media as single media is used for all type of components.
    3. Reduction in labour cost by 50%